The iron and steel industry is an important pillar industry of the national economy and the material basis for the development of the national economy and national defense construction. From the construction of large-scale projects to the manufacture of high-end tools, steel is indispensable. The level of the metallurgical industry is also a measure of a country’s industrialization, and the renewal and development of the steel industry can also directly promote the performance upgrade or technological reform of equipment in other industries. Ironmaking is an important link in steel smelting, and the molten iron produced by it is directly used in the subsequent steelmaking process. Blast furnace ironmaking is currently the most mature and common ironmaking process in the world. The tapping channel is an important part of the blast furnace tapping system. The produced high-temperature molten iron and slag flow out of the blast furnace and flow to the next process link. At the same time, depending on the density of slag iron, the tapping channel also has the function of separating molten slag and molten iron. Due to the intermittent physical erosion and chemical erosion of the slag iron, the refractory material on the iron trench needs to have higher high temperature strength and strong corrosion resistance. With the development of large-scale blast furnace smelting technology, the temperature of molten iron is higher, the amount of iron passing is more, and the time of passing iron is longer. This makes the erosion, wear and erosion of hot iron and molten slag to the tap groove more serious. Tiegou refractories put forward more stringent requirements.

At present, Al2O3-SiC-C castables are commonly used in large-scale blast furnace iron trough refractories, which have good high-temperature strength, erosion resistance and slag-iron corrosion resistance, and a long service life. Al2O3-SiC-C castables mainly contain corundum, silicon carbide, carbon materials, binders and antioxidants and other additives. Larger particle diameter corundum, silicon carbide, etc. form the aggregate of the material. When it comes to the skeleton function; other raw materials of smaller particle size form the powder of the material and fill the voids of the aggregate; the binder is mostly aluminate cement, which tightly combines the raw materials to improve the strength of the castable; more antioxidants It is metal silicon powder or aluminum powder, which is used with other additives to improve the specific properties of the castable.

After the micron-sized metal silicon is added to the castable, it can be oxidized before the easily oxidized carbon material, forming stable metal oxides and carbides, preventing the carbon material from being oxidized, so that the added carbon material is stable Play its due role and enhance the performance of castables. Generally, the amount of silicon metal added to Al2O3-SiC-C castables is between 1% and 3%. Scholars have studied the influence of the amount of silicon metal added in this interval on the properties of the castable, but its added amount Too much will affect the high temperature strength, linear change and linear expansion coefficient of the castable, thereby affecting the thermal shock stability and slag resistance of the material. This article comprehensively studies the influence of the amount of metal silicon on the physical parameters of the castable, which has certain theoretical guiding significance for the practical production of the castable.





