Dec 29, 2020 Leave a message

How To Solve The Black Spot And Cold Material Of Injection Product?

(1) Molding raw materials do not meet the requirements.

If the forming raw materials are mixed with impurities in the process of packaging, transportation, preheating and pre-drying, etc., or the raw materials of different grades are mixed with, the grain size of the raw materials is uneven or too large, the molding parts will contain foreign bodies and impurities.

In this regard, foreign bodies should be screened out of the raw materials, the choice of uniform particle size of the raw materials.

During the pretreatment and forming process, dust and other foreign matter and impurities should be prevented from mixing into the melt from the hopper, barrel and mold.

(2) Improper control of process conditions.

PVC

The causes and treatment are as follows:

A material temperature is too low, melt plastic bad.

The temperature of the barrel should be raised appropriately.

B material temperature is too high or the molding cycle is too long, melting decomposition deterioration.

The material should be reduced and the molding cycle should be shortened.

Mold C and nozzle temperature too low to produce cold particles.

The temperature of the mold and nozzle should be raised appropriately.

D injection molding machine has insufficient plasticizing capacity, and the plasticizing capacity is close to the weight of the plastic parts, making the molding time very short.

Change to a larger injection molding machine.

PEVC

E die structure is not reasonable.

If there is no cold material hole or improper positioning in the main and shunt channels of the mold, the cold material will form a rigid block in the mold when it enters the cavity.

In this regard, cold material hole should be added.

For direct feed mold, because there is no cold feed hole, cold feed spot often appears in the mold.

In this case, the cold material must be removed from the nozzle before the die is closed during operation.

When the mold is taken, the remaining cold material in the main runner should be removed to avoid cold material entering the cavity.